Thursday, October 11, 2007

Re: Both face should have Shrinkage Steel in 12 inch thick Structural Slab (ACI318)

it depends on whether it is 1 way or 2 way, you might want to read ACI 7.12
 
bart

----- Original Message -----
From: "Sanjay Verma"
To: seaint@seaint.org
Subject: Both face should have Shrinkage Steel in 12 inch thick Structural Slab (ACI318)
Date: Thu, 11 Oct 2007 11:00:46 -0700

Should 12 inch thick Structural Slab receive temperature and Shrinkage steel in both face?

 

ACI350 says about 24 in section to receive double layer of Shrink/Temp.

 

ACI 318 appears silent on this.

 

Best Regards,

Sanjay Kumar Verma,  P.E.

 



Bart Needham, SE Principal, nbse associates, inc. civil & structural engineers Office 206-780-6822 Office 805-452-8152 Fax    206-780-6683 Fax    208-693-3667 Mobile 206-300-2346  Office locations: 629 State Street #230 Santa Barbara, CA  93101  205 Fairview Lane Suite 100 Paso Robles, CA  93446  365 Ericksen Ave. NE Suite 328 Bainbridge Island, WA  98110  Mail and Deliveries: 321 High School Rd. NE Suite D-3 PMB 216 Bainbridge Island, WA  98110